The building code defines a roof coating as a fluid-applied, adhered coating used to maintain or repair a roof, or as part of a roof system. Commercial roof coatings are elastomeric: once cured they stretch to at least twice their length and recover, so they move with the roof. They renew the surface of a sound, dry roof without tearing it off; they don't fix a wet or failed one.

Coating types compared

The 2021 International Building Code lists a material standard for each common coating type: acrylic, silicone, moisture-cured polyurethane and several asphalt coatings. SEBS rubber coatings have no standard of their own.

CoatingASTM standardWhat it isPonding water
SiliconeD6694One-part silicone that cures with moisture in the air; sold solvent-free or solvent-borneMakers say it withstands ponding water
AcrylicD6083Water-based acrylic latex that dries as the water evaporatesNot for ponding water, its makers say
PolyurethaneD6947Tough urethane, usually an aromatic base coat under an aliphatic top coatThe federal spray foam spec rates it for moderate ponding
SEBSNone; IKO tests its SEBS coating to D6083Synthetic rubber (styrene ethylene butylene styrene) for metal and asphalt roofsIKO says it resists ponding better than acrylics
Asphalt and aluminumD1227, D2824 and othersAsphalt emulsions and aluminum-pigmented asphalt coatingsASTM D1227 is for slopes of at least 1/2 inch per foot

What a coating does

A coating is bonded to the roof, so it has to move with the membrane under it or it cracks and lets go. A 2001 paper in IIBEC's journal calls that tolerance for movement what separates an elastomeric roof coating from house paint, and the Department of Energy warns that ordinary paints aren't made to last on roofs.

Once cured, the manufacturers' association (RCMA) says, the coating forms an elastic film that adds waterproofing and can bridge small cracks and membrane seams. It doesn't replace repairs: leaks have to be found and fixed before coating, and RCMA says not to expect a coating to find and seal them.

DOE's 2010 guide to cool roofs names acrylic, silicone and urethane as the major coating types. It describes acrylic as water-based and very sensitive to weather while it goes on, silicone as weathering very well but weaker in tensile strength, and urethane as 3 to 10 times stronger than acrylic but harder to work with.

Is the roof a candidate?

A roof is a candidate when its membrane is sound and dry and needs its surface renewed. Gaco limits its coatings to roofs in that condition, and an article in NRCA's Professional Roofing calls a mechanically and structurally sound, dry roof a suitable candidate. DOE's guide says a coating may be a good option for a roof in good condition, with few, easy-to-repair leaks and at least five years of expected service life; a roof near the end of its life is more likely a candidate for a recover or replacement.

Coating specifications prepare a roof in roughly this order:

  1. Survey for trapped moisture. The federal coating spec names infrared, nuclear and capacitance surveys; Gaco requires a nuclear or infrared scan, and Sika makes an infrared scan mandatory over insulated roofs.
  2. Replace wet insulation. Gaco removes saturated insulation down to the deck; Progressive Materials replaces wet areas and allows moisture relief vents only for areas under 500 sq ft with moderate moisture.
  3. Repair open seams, tears and cuts with materials the membrane maker recommends, so water can't get in during the work.
  4. Clean it. Progressive Materials pressure washes at 2,000 psi or more and Gaco at more than 3,000, and the federal spec and RCMA warn against pressure that damages the roof or its seams.
  5. Test adhesion: at least three tests on each type of surface in the federal spec, which says not to go ahead until adhesion is met.
  6. Prime where the roof needs it. RCMA and the NRCA article both say a primer is no substitute for thorough cleaning.
  7. Fix drainage. The federal spec checks for ponding areas first, and EVERROOF has low areas leveled or given more drains.

When to replace instead

The same NRCA article says to tear off and replace sections where a metal roof is badly rusted or seams have failed and let water get trapped under the membrane. Gaco disqualifies thermoplastic membranes that have shrunk or gone brittle, and excludes gravel-surfaced built-up roofs.

RCMA says ballasted and gravel-surfaced roofs generally aren't acceptable surfaces for coating without special treatment, and Gaco doesn't recommend its silicone over cold-storage buildings, where constant vapor drive can trap moisture in the roof.

Ponding water

NRCA's test for proper drainage is no ponding water 48 hours after a rain in drying weather. It calls short-term ponding unavoidable but says ponding beyond 48 hours can harm the roof. The building code defines positive roof drainage the same way: enough slope that the roof drains within 48 hours.

Coatings differ here. RCMA says some are designed to withstand ponding and others aren't, and that every roof should drain. Silicone makers say theirs withstand ponding water, while acrylic makers say theirs aren't for it.

Warranties vary too. Sika notes that many roof warranties don't cover ponding water, Polyglass excludes damage from a lack of positive drainage except under its named silicones, and Gaco advertises silicone labor-and-material warranties with no ponding exclusion.

Building codes

The 2021 International Building Code added a section on roof coatings: a coating applied to a roof covering must meet the code's fire-classification rules, and coating materials must meet the standards in its Table 1509.2. NRCA proposed the change.

A coating can go over many existing roofs without a tear-off. The code's reroofing section allows a new protective coating over an existing coating, metal roof panels, built-up roofing, spray foam, metal shingles, mineral-surfaced roll roofing, modified bitumen and single-ply roofs. Since 2018, NRCA notes, a new coating doesn't count as a roof layer toward the two-layer limit.

The code doesn't allow a recover where the existing roof is water soaked or too deteriorated to serve as a base. A recover of a low-slope roof doesn't have to meet the 1/4-inch-per-foot slope required of new roofs if the roof has positive drainage.

Fire ratings belong to the tested roof assembly. The code requires classified roofs to be tested to ASTM E108 or UL 790, and NRCA says a coating has to be included in the assembly's fire listing to comply. One ICC Evaluation Service report, for example, rates an acrylic coating Class A only over 60-mil mechanically fastened TPO on a concrete or steel deck up to 2:12.

NRCA says coating standards generally require the packaging to show which standard a product meets, and fire-rating agencies require their label on listed products. In 2019 it reported that a notable number of coatings on the market lacked those markings.

Under the 2021 energy code (IECC), a roof recover doesn't have to meet new-construction energy rules as long as the building's energy use doesn't go up, while a roof replacement on a roof insulated above the deck has to meet the insulation rules. Ask the local code official how it treats a coating.

Reflectance and cool roof rules

The Cool Roof Rating Council, a nonprofit founded in 1998, rates roofing products' solar reflectance and thermal emittance. Its directory lists each product's values new and after three years of outdoor exposure at test farms in Arizona, Ohio and Florida; lab-aged Rapid Ratings stand in until the three years are up. Manufacturers pay annual fees to take part.

The council says a rating isn't a ranking or an approval, and a listing doesn't make a product cool under any code. It also warns that a thin coat over a rough surface may reflect less than the tested value.

White coatings lose reflectance as they get dirty and weather, mostly in the first year or two, DOE says. Among the white coatings on our coating pages, rated values after three years range from 0.67 to 0.69 for the silicones, 0.69 to 0.81 for the acrylics and 0.67 to 0.76 for the urethane top coats.

The 2021 IECC requires low-slope roofs over cooled spaces in climate zones 0 through 3 to meet one of the options in its Table C402.3, all based on 3-year aged ratings, such as an aged solar reflectance index of 64. Roof areas under solar panels, rooftop equipment and walkways are exempt.

California's 2025 energy code requires low-slope roofs on new nonresidential buildings, in every climate zone, to have an aged solar reflectance of at least 0.63 and thermal emittance of 0.75, or an SRI of 75. It applies to recoating too, when the smaller of half the roof or 2,000 sq ft is recoated, and products must be rated and labeled by the Cool Roof Rating Council.

EPA ended ENERGY STAR for roof products on June 1, 2022, so an ENERGY STAR claim on a roof coating is out of date.

A white roof isn't right everywhere. The federal spray foam roofing spec warns that poorly designed cool roofs in ASHRAE climate zones 4 and up have caused condensation under the membrane, and that above about R-24 of insulation a cool surface has little effect on energy use.

Coating warranties

Coating makers sell two tiers. A material-only warranty replaces defective coating but doesn't cover labor or workmanship. A labor-and-material system warranty, often no-dollar-limit (NDL), covers repairs without a cap on cost, within its terms. American WeatherStar and Polyglass both offer the two.

The term depends on dry thickness. Progressive Materials asks for 25, 30, 35 and 40 dry mils over modified bitumen for 5-, 10-, 15- and 20-year warranties, and Sika 23, 31 and 38 mils on its silicone for 10, 15 and 20 years. Each coating page lists more makers' numbers, and the coating calculator turns dry mils into gallons.

System warranties go through the maker's approved applicators and usually need approval before work starts. Sika gives jobs that weren't registered first only a 1-year material warranty and limits roofs under 5,000 sq ft to material-only coverage. The federal coating spec, Progressive Materials and Sika all call for a final inspection, which in the federal spec includes checking dry thickness.

Read the exclusions. Polyglass's sample excludes traffic or materials stored on the roof, structural movement and condensation from a missing vapor retarder; Momentive's excludes defects in the roof underneath, damage from poor drainage, and damage caused by solar panels or other equipment on the roof.

Warranties also depend on upkeep. Polyglass voids coverage if its maintenance guidelines aren't followed, Momentive requires a maintenance agreement and walkways where there's regular foot traffic, and RCMA recommends inspecting the roof twice a year and after major storms. Sika warns that adding equipment such as solar panels without consulting the manufacturer will almost always void a roof warranty.

The federal coating spec requires a no-dollar-limit warranty covering the whole system's watertightness, and its notes say not to choose more than 10 years over an existing roof; 20 years calls for a 60-mil system.

SEBS and asphalt coatings

SEBS (styrene ethylene butylene styrene) is a synthetic rubber. IKO sells a SEBS coating for restoring low-slope roofs over granule-surfaced modified bitumen and galvanized metal, and American WeatherStar sells one for metal buildings with visible rust. No coating standard in the building code covers SEBS; IKO reports its results from ASTM D6083 testing, the acrylic standard.

Asphalt coatings have their own standards: ASTM D1227 for emulsified asphalt on built-up roofs sloped at least 1/2 inch per foot, and ASTM D2824 for aluminum-pigmented asphalt. DOE says aluminized asphalt emulsions fall short of cool roof standards on low-slope roofs.

Coating guides

Roof systems

Calculator

Sources

  1. International Code Council, 2021 International Building Code, Chapter 2: Definitions
  2. Insurance Institute for Business & Home Safety (section by the Spray Polyurethane Foam Alliance), RICOWI Roof Guide: Spray Foam
  3. Gaco (Amrize Building Envelope), Application Specification ASP-S2000-22-10: GacoFlex S2000 Elastomeric Silicone Coating for Restoring Modified Bitumen and Smooth Built-Up Roofing (rev. 05/2020)
  4. NRCA, Professional Roofing, Considering coatings (Bill Kirn of National Coatings and Jim Leonard of the Reflective Roof Coatings Institute, December 2006)
  5. International Code Council, 2021 International Building Code, Chapter 15: Roof Assemblies and Rooftop Structures
  6. Roof Coatings Manufacturers Association (the manufacturers' trade group), FAQs
  7. IKO Commercial, HyKote 1000 SEBS Roof Coating product data sheet (10-RF-WH-05, January 2026)
  8. ASTM International, ASTM D6694/D6694M-25, Standard Specification for Liquid-Applied Silicone Coating Used in Spray Polyurethane Foam Roofing Systems
  9. Gaco (Amrize Building Envelope), Product Data Sheet: GacoFlex S42 Series High-Adhesion 100% Silicone Coating (rev. 07/2026)
  10. Momentive Performance Materials, Enduris 3500 Silicone Roof Coating Technical Data Sheet (07/23/2025)
  11. American WeatherStar, Product Data Sheet: Silicone 410 (PDS-092723)
  12. Gaco (Amrize Building Envelope), Product Data Sheet: GacoRoof GR16 Series Silicone Roof Coating (revised 10/2022)
  13. Henry Company, Technical Data Sheet: 887 Tropi-Cool 100% Silicone White Roof Coating (rev. 05/03/2022)
  14. ASTM International, ASTM D6083/D6083M-24, Standard Specification for Liquid-Applied Acrylic Coating Used in Roofing
  15. U.S. Department of Energy, Building Technologies Program, Guidelines for Selecting Cool Roofs, July 2010, V. 1.2
  16. Gaco (Amrize Building Envelope), Product Data Sheet (PDS): GacoFlex A47 Series Acrylic Roof Coating (Revised 12/2022)
  17. Sika Corporation, Product Data Sheet: Sikalastic-515 AC Acrylic Roof Coating (November 2025)
  18. ASTM International, ASTM D6947/D6947M-16(2023), Standard Specification for Liquid Applied Moisture Cured Polyurethane Coating Used in Spray Polyurethane Foam Roofing System
  19. USACE / NAVFAC / AFCEC, via the Whole Building Design Guide, UFGS 07 57 13 Sprayed Polyurethane Foam (SPF) Roofing (August 2025)
  20. American WeatherStar, SEBS 310 Product Data Sheet (PDS-102325)
  21. ASTM International, ASTM D1227/D1227M-13(2024), Standard Specification for Emulsified Asphalt Used as a Protective Coating for Roofing
  22. ASTM International, ASTM D2824/D2824M-18(2024), Standard Specification for Aluminum-Pigmented Asphalt Roof Coatings, Nonfibered, and Fibered without Asbestos
  23. IIBEC, Interface (William A. Kirn, Rohm and Haas), ASTM D-6083 Standard Specification for Liquid Applied Acrylic Coating Used in Roofing: What It Says, What It Means, How It Came to Be (January 2001)
  24. Roof Coatings Manufacturers Association (the manufacturers' trade group), About Roof Coatings
  25. USACE / NAVFAC / AFCEC, via the Whole Building Design Guide, UFGS 07 56 00.60 Mesh Reinforced Elastomeric Coating (MREC) Roofing (August 2025, Change 1 February 2026)
  26. Sika Corporation, RoofCoat Project Warranty Registration form (01/2026)
  27. Progressive Materials (PM Silicone), Recommended Design Specification: Silicone Roof Coating Restoration System over Modified Bitumen, Cap Sheet, or Smooth Surface BUR (August 2025)
  28. EVERROOF Products, Applications Guide, Roll: Roof Maintenance Coating Systems
  29. NRCA, Professional Roofing, Still water runs deep (Jason Wilen, July 2012)
  30. Sika Corporation, 6 Key Factors in Assessing Low Slope Roof Warranties
  31. Polyglass U.S.A., Inc., 15 Year Coating System Limited Non-Prorated, No Dollar Limit Warranty, with Owner Maintenance Guidelines (sample)
  32. Gaco (Amrize Building Envelope), GacoFlex S42 family brochure (2025)
  33. NRCA, Professional Roofing, Roof coatings and code compliance (Mark S. Graham, September 2022)
  34. NRCA, Professional Roofing, Coating concerns (Mark S. Graham, March 2019)
  35. ICC Evaluation Service, ESR-5000: NanoTech Materials Cool Roof Coat (reissued June 2026)
  36. International Code Council, 2021 International Energy Conservation Code, Commercial Provisions, Chapter 5: Existing Buildings
  37. Cool Roof Rating Council, About the CRRC
  38. Cool Roof Rating Council, Rated Products Directory, roof products: headings and disclaimers
  39. Cool Roof Rating Council, Roof Rating Program
  40. U.S. Department of Energy (Lawrence Berkeley National Laboratory presentation), Stay-Clean and Durable White Elastomeric Roof Coatings (2014 Building Technologies Office peer review)
  41. Cool Roof Rating Council, Rated Products Directory, roof products (downloaded October 18, 2026)
  42. Cool Roof Rating Council, Rated Products Directory: Tremco Solargard 1120 White, 0612-0012
  43. Cool Roof Rating Council, Rated Products Directory: Sikalastic 515 AC, 0674-0046
  44. Cool Roof Rating Council, Rated Products Directory, roof products (downloaded October 18, 2026)
  45. International Code Council, 2021 International Energy Conservation Code, Commercial Provisions, Chapter 4: Commercial Energy Efficiency
  46. California Energy Commission, 2025 Energy Code: Nonresidential Cool Roofs (Energy Code Support Center)
  47. U.S. Environmental Protection Agency (ENERGY STAR), ENERGY STAR Roof Products Sunset Decision Memo (letter dated May 28, 2019)
  48. U.S. Environmental Protection Agency (ENERGY STAR), ENERGY STAR Roof Products Sunset Reminder
  49. American WeatherStar, Warranty Program
  50. Polyglass U.S.A., Inc., Coating Material Only Limited Warranty (sample)
  51. Sika Corporation, Sikalastic RoofCoat Warranty Process
  52. Momentive Performance Materials, GE Enduris Roof Restoration Coating Product Plus Warranty, with Owner Care & Maintenance Information (sample, 2022)